We manufacturer Compressibility and Recovery Tester as per ASTM F 36.

Technical Specification:
  • Area of specimen to be tested: 40 mm2
  • Diameter of test specimen: 22.6 mm
  • Diameter of indenter: 25 mm
  • Range of thickness measurement: 0 – 19 mm x 0.01 mm
  • Initial load on test specimen: 7 kPa (286 g)
  • Final load on test specimen: 2800 kPa (114 kg)
  • Range of spring dynamometer: 150 kg